Thickness Tolerance
(Unit : mm)
Process | Thickness(mm) | Tolerance | Diametrical Variation |
---|---|---|---|
HD, RAIP, (S)AIP, SAIP, PASAIP, PSASAIP |
3.00 Under 3.01~6.00 6.01~10.00 10.01~18.00 18.01 Over |
+0, -0.020 +0, -0.025 +0, -0.030 +0, -0.040 +0, -0.050 |
MAX 0.010 MAX 0.013 MAX 0.015 MAX 0.020 MAX 0.025 |
Form | ~6.00 6.01~18.00 18.01 Over |
±0.05 ±0.08 ±0.10 |
MAX 0.020 MAX 0.025 MAX 0.030 |
tetragonal, pentagonal, hexagonal, etc |
Surface Defect
(Unit : mm)
Process | Thickness(mm) |
---|---|
RAF, (S)AF, SAF, PASAF | 0.05 Below |
(S)AIP, SAIP, PASAIP, PSASAIP | 0.05 Below |
Spheroidization Rate
(Unit : %)
Classification | Spheroidization Rate |
---|---|
RAF, RAIP, (S)AIP | 70±10 |
SAF, SAIP | 80 More than |
PASAF, PASAIP, PSASAIP | 90 More than |
Decarburized Layer Depth
(Unit : mm)
Thickness(mm) | FERRITE Decarburization Depth(DMF) | TOTAL Decarburization Depth(DMT) |
---|---|---|
8.00 Under | Max 0.02 | Max 0.08 |
8.01~14.00 | Max 0.03 | Max 0.10 |
14.01~20.00 | Max 0.04 | Max 0.12 |
20.01 Over | Max 0.05 | Max 0.18 |